Polymer Process Aids

(PPA)

Product Details

 

 

Physical Property :

 

ITEM

UNIT

SETTING

Aluminum Content

(%)

1.30-1.70

Phosphorus Content

(%)

2.50-3.70

Whiteness

(R457)

>90%

 

 

Product Form :

 

      ◾️    White to off-white powder

 

 

Product application :

 

      ◾️    Unreinforced nylon, reinforced nylon, glass fiber reinforced nylon.

 

 

Processing Guide :

 

      ◾️    It is recommended to add 0.1%-0.3% of T22 to obtain the best performance . The specific addition amount is added as appropriate

             according to the volume of nylon and the expected requirements of specific products . 

 

 

Product Functions :

 

      ◾️    Shorten molding cycle and improve production efficiency ;

      ◾️    Improve mold release ;

      ◾️    Improve product dimensional stability ;

      ◾️    Increase tensile strength and hardness .

 

 

Packaging & Storage :

 

      ◾️    10KG/CARTON. 500KG/PALLET .  

      ◾️    Store in cool dry and sun block condition .

Nucleating Agent T22

ADDYNCA Nucleating Agent T22 is a special nucleating agent for polyamides. 
It is easy to be dispersed, to promote the crystallization speed of resins, improve the crystallinity and improve the processing and application performance of products.